Hautojärvi, P. (1981). Points defects in amorphous Fe[sub 80] B[sub20] and Fe[sub 40] Ni[sub 40] P[sub 14] B[sub 6] studied by positron lifetime and magnetic after-effect. [Helsinki University of Technology].

Chicago Style Citation

Hautojärvi, P. Points Defects in Amorphous Fe[sub 80] B[sub20] and Fe[sub 40] Ni[sub 40] P[sub 14] B[sub 6] Studied by Positron Lifetime and Magnetic After-effect. [Espoo]: [Helsinki University of Technology], 1981.

MLA Citation

Hautojärvi, P. Points Defects in Amorphous Fe[sub 80] B[sub20] and Fe[sub 40] Ni[sub 40] P[sub 14] B[sub 6] Studied by Positron Lifetime and Magnetic After-effect. [Helsinki University of Technology], 1981.

Harvard Style Citation

Hautojärvi, P. 1981. Points defects in amorphous Fe[sub 80] B[sub20] and Fe[sub 40] Ni[sub 40] P[sub 14] B[sub 6] studied by positron lifetime and magnetic after-effect. [Espoo]: [Helsinki University of Technology].